- Spruce (Satin), Oak (Satin), Larch (Satin), Douglas Fir (Satin), Cedar (Satin), Natural (Satin), Light Red Cedar (Satin), Light Oak (Satin)
Wood surface must be clean, dry and frost-free (moisture content max. 20%). UV-Protection-Oil Tints is ready to use. Do not thin. Stir well using a flat stirring stick or spatula before use. Ideally, surfaces are sanded no finer than a P120 grit grade of sand paper. Sanding to finer grades will reduce required absorbency.
If possible, and if the wood is absorbent, please apply first coat to all sides before installation. Fresh wood containing natural wood ingredients /extractives (eg: Cedar, Teak, Mahogany or Iroko) are often less absorbent and need to weather off first before applying the product. Please refer to website ‘Suitability’ section for more details. Weathering helps ingredient rich wood become more absorbent and the wood finish adheres optimally.
For renovation works, clean old microporous stains thoroughly – if necessary sand lightly. Clean and restore already greyed or weathered wood at the same time with Osmo Wood Reviver Power-Gel. Old paints and lacquers must be completely removed. As a general rule, wear a dust mask during sanding works. To maintain absorbency, avoid sanding surfaces finer than a P120 grit. Weather ingredient rich wood after sanding.
The finished surface is influenced by several factors, including the condition of the wood. Therefore, a trial application is always required, especially for unfamiliar surfaces.
Soft wood species like Pine or Spruce are more prone to blue stain, rot and insects. If desired, pre-treat these soft woods if possible on all sides with Osmo WR Base Coat.
For all other wood types not mentioned, always trial apply first.
For the following wood types, WR Base Coat is recommended before use.
For the following wood types, a weathering period is recommended. New or sanded wood requires at least 12 weeks (approximate) exposure to the exterior elements before application.
After the weathering period, it’s generally recommended to de-grey the surface with Osmo Wood Reviver Power-Gel and clean the surface from the extractive content before application, always trial apply!
For all other ingredient-rich hardwood species not mentioned may require a varied period of exposure. Please contact us for further information.